Surface scratches under the paint film.
Cause
Shrinkage of the paint film during drying causes it to follow the contours of any scratches or other finishing marks in the underlying surface. The defect results from:
Prevention
Rectification
If the marks are light it may be sufficient to flat, compound and polish the affected area. In more severe cases the surface must be rubbed down until the marks are removed and then repainted.